Just before a board enters the reflow oven, its surface-mount components are already in place. Their terminals rest on deposits of solder paste. Follow one of those connections through the oven to see how the paste becomes a solid joint between a terminal and a PCB pad.
A stencil transfers solder paste onto selected pads on the bare printed circuit board. The paste contains fine particles of solder alloy mixed with flux. When the placement machine sets a component onto the deposits, the tackiness of the paste helps hold the part in place for the trip to the oven.
The position of the paste and the position of the terminal both matter. Printing puts the solder where it is needed. Placement brings the two surfaces together. The RONGHE factory tour shows how printing, placement, and reflow fit into the surface-mount assembly sequence.

Solder paste printing and inspection stations on the RONGHE SMT line.
As the assembly warms, the flux helps remove oxides from the solder particles and the surfaces to be joined. Some thermal profiles include a period called a soak to reduce temperature differences across the assembly. The choice depends on the board, the parts, and the solder paste.
Once the alloy is above its liquidus temperature, it is fully molten. It can spread over the solderable surfaces of the pad and terminal, a process called wetting. As the board cools, the solder solidifies. The resulting joint electrically connects the terminal to the pad and mechanically secures the component. For more on the heating and cooling stages, see Indium Corporation’s guide to reflow phases.

The same terminal and pad before reflow, during wetting, and after the solder has solidified.
Oven zone settings and conveyor speed influence how the board heats up, but they give engineers only part of the picture. A location near a large copper area can heat differently from a small pad elsewhere on the same board. Engineers can attach thermocouples at selected locations on a representative assembly to record the temperature each location actually reaches over time.
Those measurements form the reflow profile. Engineers use it to check how quickly the board heats and cools, how hot it gets, and how long the solder remains above its liquidus temperature at the measured locations. The solder paste supplier’s recommendations and the limits of the components both matter when selecting a profile. Texas Instruments’ assembly application note explains this approach for QFN and SON packages.
When a board comes out of reflow, the solder joints are formed and the assembly can move on to inspection. Automated optical inspection can examine visible assembly features. Functional testing answers a separate question about how the assembled board behaves under defined conditions. See what AOI and functional testing can verify or follow the full control board manufacturing process.
It is the time a measured location spends above the temperature at which the solder alloy is fully liquid. It is one part of the temperature history used to evaluate the reflow profile.
Board construction, copper distribution, and component layout can change how heat reaches different locations. The solder paste and the components also have their own process limits.
Explore custom PCB and PCBA manufacturing or contact RONGHE about your assembly project.